ASTM B574 Alloy N6022 C-22 Grade:
Mechanical Property Requirements for Hot or Cold Finished, Solution Annealed Rods
ASTM B574 Alloy N6022 C-22 Grade: Chemical Composition
Element | Composition (%) |
---|---|
Carbon (C) | 0.010 max |
Chromium (Cr) | 20 – 22.5 |
Cobalt (Co) | 2.5 max |
Iron (Fe) | 2.0 – 6.0 |
Manganese (Mn) | 0.50 max |
Molybdenum (Mo) | 12.5 – 14.5 |
Nickel (Ni) | Balance |
Phosphorus (P) | 0.02 max |
Silicon (Si) | 0.08 max |
Sulfur (S) | 0.02 max |
Tungsten (W) | 2.5 – 3.5 |
Vanadium (V) | 0.35 max |
ASTM B574 Alloy N6022 C-22 Grade: Mechanical Properties
Product Form | Tensile Strength (ksi [MPa]) | 0.2% Yield Strength (ksi [MPa]) | Elongation (%) | Hardness (HRb) |
---|---|---|---|---|
Bars/Rods | 100 [690] | 45 [310] | 45 | 89 |